Made to order
- COA on request — PSD, sphericity, flow rate, chemistry
- Mutual NDA before any file or spec review
A-Powder Inconel 718 Nickel Alloy Powder for LPBF — 15–53 µm, 10 kg
A-Powder Inconel 718 powder price: $835 per 10 kg ($83.50/kg)
Age-hardenable nickel superalloy with excellent strength at high temperature and good corrosion resistance. A-Powder is AO Metal's own powder brand, produced in China and sold and supported in the US by Additive Plus.
Values from the manufacturer data for A-Powder Inconel 718. Catalog figures are minimums or ranges; the certificate for your lot is available on request.
Which Inconel 718 is right for your build?
All of them are in our catalog at a published price. Pick by machine, timing and country of origin.
| Powder | Particle size | Origin | Availability | Good fit for | 10 kg | |
|---|---|---|---|---|---|---|
| 15–45 µm · LPBF | USA | Out of stock | Programs that need a named mill and fast delivery | $1,000 | View | |
| 45–106 µm · DED, EBM | Confirmed per lot | In stock | Directed energy deposition and electron-beam systems | $575 | View | |
| 15–53 µm · LPBF | China | Made to order | R&D and cost-driven builds that can wait | $900 | View | |
| 15–53 µm · LPBF | China | Made to order | Lower LPBF price per kg, made to order | $835 | Add to cart |
Need a specific country of origin for a government or defense program? Ask before ordering and we will confirm it in writing for your lot.
What is in the container
Specification from the manufacturer. The certificate for your lot is available on request.
Specification
Chemistry, manufacturer data for A-Powder Inconel 718 (wt%). The certificate for your lot lists all measured elements.
| Element | wt% |
|---|---|
| Nickel (Ni) | 50.0–55.0 |
| Chromium (Cr) | 17.0–21.0 |
| Niobium (Nb) | 4.75–5.5 |
| Molybdenum (Mo) | 2.8–3.3 |
| Iron (Fe) | Balance |
| Powder property | Requirement |
|---|---|
| D10 / D50 / D90 | 10–25 / 25–40 / 40–60 µm |
| Hall flow | ≤ 20 s / 50 g |
| Apparent / tap density | ≥ 3.5 / ≥ 4.0 g/cm³ |
| Sphericity | ≥ 80% |
What comes with your lot
From the manufacturer certificate
- Chemistry against the specification limits on the left
- Particle size distribution: D10, D50, D90
- Flow rate and apparent density
- Lot number for traceability
The certificate for your lot is available on request. The manufacturer datasheet for this alloy has no particle image; ask us if you need one.
How the printed metal performs
Printed-property minimums from the manufacturer data for A-Powder Inconel 718. A guide for your own qualification, not design data.
| Condition | Orientation | Yield, MPa | UTS, MPa | Elongation | Rel. density | Hardness, HV1 |
|---|---|---|---|---|---|---|
| As-built | — | ≥ 829 | ≥ 1049 | ≥ 27% | 99.82% | 286 |
| 1065 °C 8 h + 720 °C 4 h + 620 °C 4 h | — | ≥ 1307 | ≥ 1458 | ≥ 17% | — | 530 |
Heat treatment
Manufacturer data
- Heat treatment in the catalog data: 1065 °C for 8 hours, then 720 °C for 4 hours and 620 °C for 4 hours.
- Use the solution, aging and HIP cycle your specification calls for, for example AMS5662.
Before you order
Ship date: confirmed by email after you order. If it does not work for you, we cancel the order and refund it in full.
How this Inconel 718 compares
Published tensile data, X–Y direction unless noted, one representative condition per alloy. Conditions differ, so use this to shortlist, not to design.
| Alloy | Condition | Yield, MPa | UTS, MPa | Elongation | Choose it for | 10 kg |
|---|---|---|---|---|---|---|
| Inconel 718 | 1065 °C 8 h + 720 °C 4 h + 620 °C 4 h (manufacturer data) | ≥ 1307 | ≥ 1458 | ≥ 17% | Lowest price per kg | $835 |
| Inconel 625 | Stress relieved | 648 | 1007 | 41% | Corrosion resistance; cryogenic to 1093 °C (2000 °F) | $1,160 |
| Hastelloy X | Solution + age | 393 | 816 | 41% | Oxidation resistance to 1204 °C (2200 °F) | $1,125 |
Will it run on my printer?
Runs on open-parameter laser powder bed fusion systems with Inconel 718 parameters. Our materials engineer shares recommended starting parameters that you tune on your machine.
AO MetalA30 · A50 · A100Benchtop to production LPBF with open parameters. Ask our materials engineer for starting parameters.From $59,000 · A30See AO Metal printers →
FarsoonMetal LPBF lineOpen-platform LPBF from compact R&D frames to 16-laser production systems.FS121M · FS191M · FS200M · FS273M · FS301M · FS350M · FS422M · FS621M · FS721M · FS812M · FS1311M · FS1521MQuote on requestSee Farsoon metal printers →Machine names identify compatible equipment only. Additive Plus is not affiliated with these manufacturers, and the powder is not approved by them. Process parameters are tuned per machine.
Store sealed
Keep the container closed, dry and at room temperature until you load the printer.
Sieve
Sieve before loading and every time you reuse powder recovered from a build.
ATO Sieve · quoteLoad and purge
Fill the dispenser, close the chamber and purge with argon or nitrogen.
Print and relieve
Stress-relieve on the plate, then remove parts and supports.
Recover
Collect unfused powder, sieve it and return it to a sealed container.
Delfin Mistral 451 BL D2 — ATEX metal powder vacuum · $7,175Wear a respirator, gloves and eye protection when handling metal powder. Read the safety data sheet before first use.
Printed on AO Metal
Real builds on the LPBF printers we sell, and what teams make from this alloy.




Parts printed on AO Metal printers, which we sell. Alloys, parameters and powder lots differ from part to part; these photos show the process, not parts made from this specific powder lot.
- Turbine and engine parts
- Hot-section aerospace parts
- Industrial high-temperature parts
Applications as listed in the manufacturer data for A-Powder Inconel 718.
Ordering, delivery and our promise
A sealed 10 kg container of 15–53 µm powder, with the certificate of analysis for the lot on request.
The ship date shows next to the Add to Cart button. Shipping cost is calculated at checkout.
Card or PayPal at checkout, an invoice, or a purchase order — choose how you buy next to Add to Cart.
100 kg and more: ask for a volume quote with your alloy, quantity and ship-to.
If the powder is not right, we make it right.
If your lot’s chemistry or particle size falls outside its certificate or this page, or it arrives damaged or wrong, tell us within 14 days of delivery. We replace it or refund you, and we pay for shipping both ways.
Complete the workflow
- ✓ 316L — stronger pitting and chemical resistance than 304 stainless
- ✓ Precision-ground flatness for consistent first-layer adhesion
- ✓ Made to order — choose your speed below: Express 2–3 wks, or Standard 6–8 wks (save ~45%)
ATEX-certified industrial vacuum for combustible dust and non-reactive metal powder — built to the D2 standard for Zone 22 areas, with antistatic, grounded construction and a Class M filter. 2 kW, 3-inch inlet, 12-gallon container.
- ✓ Conductive / antistatic build — no static build-up around ignition-sensitive powder
- ✓ For stainless, nickel & non-reactive AM powder — reactive metals need the inert unit
- ✓ In US stock · ships in 2–3 business days · genuine Delfin unit · ATEX docs on request
Automated 2-in-1 blasting cell that depowders and surface-finishes powder-bed 3D-printed parts in one enclosed, software-controlled cycle.
- ✓ Depowdering + surface finishing in one ATEX-compliant cell
- ✓ Polymer PBF (SLS, MJF, HSS, SAF) + de-powdered metal parts
- ✓ Lead time: 4–8 weeks — built to order · install + training included
High-temp. Corrosion-proof. Non-magnetic. Genuine Carpenter PowderRange® 625 (Inconel® 625) nickel superalloy for LPBF, EBM & DED metal 3D printing.
- ✓ Strength & corrosion resistance to 2000°F (1093°C)
- ✓ Sold in small, workable volumes — no large mill minimums
- ✓ COA on request
Other alloys in US stock now
Premium-grade LPBF powders, COA on request — add to cart or request a formal quote.
Carpenter Additive · Made in USAIN939 Nickel Alloy Powder for Metal 3D PrintingIn stock · ships in ~2 business days$1,770 / 10 kg · $177.00/kg
Carpenter Additive · Made in USAHastelloy X Powder for Additive ManufacturingIn stock · ships in ~2 business days$1,125 / 10 kg · $112.50/kg
Carpenter Additive · Made in AustriaAluminum Alloy Powder AlSi10MgIn stock · ships in ~2 business days$830 / 10 kg · $83.00/kg
Carpenter Additive · Made in USAM300 Maraging Steel Powder for Metal 3D PrintingIn stock · ships in ~2 business days$945 / 10 kg · $94.50/kgCommon questions
Don't see yours? Email [email protected] — NDA on request.
What is A-Powder Inconel 718 nickel alloy powder?
What strength does printed Inconel 718 nickel alloy reach with this powder?
How is Inconel 718 nickel alloy heat treated after printing?
What particle size and flow does A-Powder Inconel 718 nickel alloy powder have?
Who makes A-Powder Inconel 718 nickel alloy powder?
How is A-Powder Inconel 718 nickel alloy powder different from PowderRange 718 from Carpenter Additive?
How do I order A-Powder Inconel 718 nickel alloy powder, and when does it ship?
Place your order, or talk to an engineer first
Order A-Powder Inconel 718 Powder for Metal 3D Printing | 15–53 µm LPBF – 10 kg / 22 lbs direct, or talk to materials engineer
Get a quote — response in under 24h
Tell us about your part. A real applications engineer reviews every quote — no contact-form roulette. NDA on request, free DfAM review for first-time customers.
Talk to an applications engineer
30 minutes with the team that designs AO Metal and runs our print services. We'll review your spec, recommend a process, and send a tailored proposal — installation, training, service included.
Book a demo with the team that built it
See the equipment running on a real part — in our L.A. shop or remotely. The engineer on the call is the one who'll support the machine after it ships.
Free DfAM review on your first order.
Real engineering review by an applications engineer — not an automated check. Claim it once per company.
- Engineer-reviewed quote within 24 hours
- Free DfAM & material recommendation
- NDA on request before file review
Claim your offer
Takes 30 seconds. We'll reply within 24h with your claim code and a quote-ready link.