A-Powder Inconel 718 Nickel Superalloy Powder for Metal 3D Printing | LPBF Compatible – 10 kg / 22 lbs

$1,090

High-Temperature Strength. Corrosion-Resistant.. High-performance Inconel 718 powder for LPBF additive manufacturing. Heat-resistant, corrosion-resistant, and fully heat-treatable for aerospace, energy, and industrial high-temperature components. OEM-optimized Inconel 718 powder for metal 3D printing, delivering reliable prints, predictable LPBF performance, and full traceable documentation.

 

  • Technology:

    Metal LPBF

  • Printing Materials:

    Metal Powders

  • Production Method:

    Vacuum Induction Melting Gas Atomization (VIGA)

  • Powder Package:

    10 kg bottle, 440 kg hopper, 840 kg hopper

  • In stock

  • Delivery: 5-10 Business Days

$1,090

Need more than 100 kg / 222 lbs? Or official request?

OEM-Optimized Supply — Powered by Additive Plus
✔ Application-driven material engineering and validation
✔ Optimized printing parameters for maximum performance
✔ Reduced trial-and-error through pre-qualified solutions
✔ Improved repeatability and process stability
✔ Developed for demanding industrial use cases

Order more than 100 kg and get a discount
Quantity, kg Per Bottle 10 kg Per kg
10-100 $1090.00 $109.00
100+ $980.00 $98.00
  • Description
  • Details
  • Materials
  • FAQ
  • Documents
  • Videos
  • Review

Description

A-Powder Inconel 718 Nickel Superalloy Powder is a premium nickel-based superalloy designed for LPBF additive manufacturing. Produced via vacuum induction gas atomization (VIGA), the powder features spherical morphology, tight particle size distribution (15–53 µm), and ultra-low oxygen content (≤200 ppm). This ensures smooth recoating, predictable flow, and repeatable layer fusion. The alloy composition (Ni 51.7 %, Cr 20.06 %, Fe balance, Nb 5.01 %, Mo 3.17 %, Ti 1.02 %, Al 0.47 %) provides excellent high-temperature strength and corrosion resistance. Heat treatment achieves ultimate tensile strength 1350 MPa, yield strength 1150 MPa, and elongation 23 %, making A-Powder Inconel 718 ideal for aerospace, energy, and critical industrial applications. Small-batch flexibility, rapid delivery, and full traceable documentation from AO Metal guarantee production-ready performance.

Element Min Max Typical
Fe Bal. Bal. Bal.
Cr 15.0 17.0 16.28
Cu 3.0 5.0 4.15
Ni 3.0 5.0 4.18
Nb+Ta 0.15 0.45 0.28
Si 1.0 0.49
Mn 1.0 0.20
C 0.07 0.006
P 0.02 0.006
S 0.02 0.004
O 0.08 0.030
N 0.15 0.015

machine type: F – LPBF INDUSTRIES: Aerospace /  Energy /  Industrial

Key Performance Benefits

  • High-temperature nickel-based superalloy with excellent corrosion resistance
  • Predictable LPBF performance with stable layer deposition
  • Spherical particle morphology ensures repeatable powder flow
  • Heat-treatable for optimized mechanical properties
  • Suitable for complex, high-temperature, end-use components

Typical Applications

  • Aerospace turbine and structural components
  • High-temperature energy and power system parts
  • Industrial machinery requiring corrosion resistance and strength
  • Precision end-use components for critical applications
  • Brand AO Metal – High-Precision Metal 3D Printers for Innovation
  • Technology Metal LPBF
  • Powder Package 10 kg bottle, 440 kg hopper, 840 kg hopper
  • PSD (particle size distribution) 15–53 micrometres
  • Printing Materials Metal Powders
  • Material IN718
  • Country of origin China
  • Production Method Vacuum Induction Melting Gas Atomization (VIGA)

Materials

Applicable Standards: ASTM F3055, ASTM B213, ASTM B212, ASTM B527, ISO13320
Manufacturing Method: Vacuum Induction Melting Gas Atomization (VIGA).
Particle Shape: Spherical.

  • IN718

Frequently asked questions

What is Inconel 718?

Inconel 718 is a nickel-based superalloy powder engineered for LPBF additive manufacturing. It provides excellent high-temperature strength, corrosion resistance, and predictable mechanical performance after heat treatment.

Which additive manufacturing processes are compatible?

Optimized for LPBF. Spherical particles with tight PSD (15–53 µm) and ultra-low oxygen content (≤200 ppm) provide smooth recoating, minimal spatter, and repeatable layer deposition.

Can Inconel 718 be heat-treated?

Yes, heat treatment improves mechanical properties: UTS 1350 MPa, yield 1150 MPa, elongation 23 %, hardness 45 HRC.

What industries typically use Inconel 718?

Aerospace, energy, and industrial applications requiring high-temperature, corrosion-resistant, and structurally critical components.

Documents

Videos