A-Powder Inconel 718 Nickel Superalloy Powder for Metal 3D Printing | LPBF Compatible – 10 kg / 22 lbs
What your process engineer actually checks
Locked, traceable lot chemistry
Every lot ships with a COA documenting PSD, sphericity, flow rate, apparent density, and full chemistry — and a lot number you can trace. Aerospace and medical teams reorder 4+ times without re-qualifying.
Qualified parameters, not just powder
Validated parameter sets for EOS M 290, Renishaw 500Q, SLM 280, and our own AO Metal LPBF ship with the order. Load the profile and hit density on the first build — no parameter-development burn.
A materials engineer on the line
Questions on ferrite content, flowability, recyclate ratios, or HIP response? A materials engineer answers directly — not a contact-form bot. Most replies in under 4 hours, NDA standard.
A-Powder Inconel 718 Nickel Superalloy Powder is a premium nickel-based superalloy designed for LPBF additive manufacturing. Produced via vacuum induction gas atomization (VIGA), the powder features spherical morphology, tight particle size distribution (15–53 µm), and ultra-low oxygen content (≤200 ppm). This ensures smooth recoating, predictable flow, and repeatable layer fusion. The alloy composition (Ni 51.7 %, Cr 20.06 %, Fe balance, Nb 5.01 %, Mo 3.17 %, Ti 1.02 %, Al 0.47 %) provides excellent high-temperature strength and corrosion resistance. Heat treatment achieves ultimate tensile strength 1350 MPa, yield strength 1150 MPa, and elongation 23 %, making A-Powder Inconel 718 ideal for aerospace, energy, and critical industrial applications. Small-batch flexibility, rapid delivery, and full traceable documentation from AO Metal guarantee production-ready performance.
| Element | Min | Max | Typical |
| Fe | Bal. | Bal. | Bal. |
| Cr | 15.0 | 17.0 | 16.28 |
| Cu | 3.0 | 5.0 | 4.15 |
| Ni | 3.0 | 5.0 | 4.18 |
| Nb+Ta | 0.15 | 0.45 | 0.28 |
| Si | – | 1.0 | 0.49 |
| Mn | – | 1.0 | 0.20 |
| C | – | 0.07 | 0.006 |
| P | – | 0.02 | 0.006 |
| S | – | 0.02 | 0.004 |
| O | – | 0.08 | 0.030 |
| N | – | 0.15 | 0.015 |
machine type: F – LPBF INDUSTRIES: Aerospace / Energy / Industrial
Key Performance Benefits
- High-temperature nickel-based superalloy with excellent corrosion resistance
- Predictable LPBF performance with stable layer deposition
- Spherical particle morphology ensures repeatable powder flow
- Heat-treatable for optimized mechanical properties
- Suitable for complex, high-temperature, end-use components
Typical Applications
- Aerospace turbine and structural components
- High-temperature energy and power system parts
- Industrial machinery requiring corrosion resistance and strength
- Precision end-use components for critical applications
| Brand | AO Metal – High-Precision Metal 3D Printers for Innovation |
| Technology | Metal LPBF |
| Powder Package | 10 kg bottle, 440 kg hopper, 840 kg hopper |
| PSD (particle size distribution) | 15–53 micrometres |
| Printing Materials | Metal Powders |
| Material | IN718 |
| Country of origin | China |
| Production Method | Vacuum Induction Melting Gas Atomization (VIGA) |
We atomize our own. Custom variants on request.
Tighter PSD, modified chemistry, custom blend? Our ATO atomization lab runs custom batches in 3–4 weeks. Biocompatible, refractory, proprietary — all in-house, verified before ship.
Other products teams run alongside A-Powder Inconel 718 Nickel Superalloy Powder for Metal 3D Printing | LPBF Compatible – 10 kg / 22 lbs
On backorder
Corrosion-Resistant. High-Temperature Stable. High-performance IN625 nickel powder for LPBF additive manufacturing. Corrosion-resistant, heat-stable, and fully heat-treatable for aerospace, energy, and industrial high-temperature components.
OEM-optimized IN625 powder for metal 3D printing, delivering reliable prints, predictable LPBF performance, and full traceable documentation.
In stock
· 5-10 Business Days
In stock
In stock
In stock
In stock
In stock
From process engineers running A-Powder Inconel 718 Nickel Superalloy Powder for Metal 3D Printing | LPBF Compatible – 10 kg / 22 lbs
Unedited feedback from customers who reorder A-Powder Inconel 718 Nickel Superalloy Powder for Metal 3D Printing | LPBF Compatible – 10 kg / 22 lbs.
Same lot 4 times in a row. We stopped re-running parameter sweeps after the second order — density was identical to the first build.
Asked about ferrite content on a Friday. A materials engineer answered Monday morning with actual data, not a sales pitch. That's why we keep ordering.
COA matches the bottle. PSD and flow are exactly what was on the sheet — we run it on a Renishaw 500Q and it hits density on the first try.
Common questions
Don't see yours? Email [email protected] — NDA standard, typical reply within 4 hours.
What is Inconel 718?
Which additive manufacturing processes are compatible?
Can Inconel 718 be heat-treated?
What industries typically use Inconel 718?
Place your order, or talk to an engineer first
Order 316L direct, or send your application and we'll recommend the right alloy and PSD for your printer.
Get a quote — response in under 24h
Tell us about your part. A real applications engineer reviews every quote — no contact-form roulette. NDA standard, free DfAM review for first-time customers.
Talk to an applications engineer
30 minutes with the team that designs AO Metal and runs our print services. We'll review your spec, recommend a process, and send a tailored proposal — installation, training, service included.
Book a demo with the team that built it
See the equipment running on a real part — in our L.A. shop or remotely. The engineer on the call is the one who'll support the machine after it ships.
Free DfAM review + free U.S. shipping on your first order.
Real engineering review by an applications engineer — not an automated check. Plus free domestic shipping, no minimum. Claim it once per company.
- Engineer-reviewed quote within 24 hours
- Free DfAM & material recommendation ($150 value)
- Free U.S. shipping (no minimum on first order)
- NDA signed before file review
Claim your offer
Takes 30 seconds. We'll reply within 24h with your claim code and a quote-ready link.