In stock
- Sealed, chip-tracked cartridge — factory-sealed with its Nexa3D lot.
- Validated LSPc profile — print settings plus wash, UV and thermal cure guidance.
Nexa3D xPRO9400-FR Flame-Retardant Engineering Resin – UL 94 V-0 at 2 mm | 1.5 kg
Halogen-free flame-retardant engineering resin — UL 94 V-0 at 2 mm with very high heat resistance, developed with BASF Forward AM.
- ✓ UL 94 V-0 at 2 mm (V-1 at 1.5 mm); rail DIN EN 45545-2 HL1/HL2; LOI ≥ 28
- ✓ Stiff and hot: 88 Shore D, HDT up to 250 °C @ 0.45 MPa (with 150 °C post-cure)
- ✓ 1.5 kg cartridge for Nexa3D XiP / XiP Pro (LSPc)
$250
What your process engineer actually checks
A flame rating tied to a wall thickness
UL 94 V-0 on xPRO9400-FR is rated at 2 mm — thinner sections are not covered by that rating, and the top heat numbers need the three-hour 150 °C thermal post-cure. We give you the cure schedule and the wall-thickness caveat up front so your compliance submission does not come back.
A materials engineer on the line
Resin selection, exposure tuning, post-cure and finishing — answered by engineers who print Nexa3D LSPc in-house. Sub-4h reply, NDA standard.
Nexa3D xPRO9400-FR is a halogen-free, flame-retardant engineering photopolymer developed with BASF Forward AM — for functional parts that must resist ignition and high temperatures, from electrical enclosures to rail interior components.
Why engineers choose xPRO9400-FR
Fire and thermal performance documented on the Nexa3D TDS.
Flame retardant
UL 94 V-0 at 2 mm (V-1 at 1.5 mm), halogen-free. Rail DIN EN 45545-2 HL1/HL2, LOI ≥ 28, low smoke per ISO 5659-2.
Very high heat resistance
HDT up to ~250 °C at 0.45 MPa (141 °C at 1.82 MPa) after a 150 °C post-cure. Glass transition 175 °C.
Rigid and strong
71–78 MPa tensile, 115 MPa flexural, 88 Shore D — plus electrical-insulator resistivity for enclosures.
LSPc workflow
Runs on Nexa3D XiP, XiP Pro, and NXE 400Pro with validated NexaX profiles. Preheat 5 h at 60 °C before printing.
From cartridge to finished part
A short thermal step unlocks the full fire and heat rating.
Preheat & print
Preheat 5 h at 60 °C, shake until clear, load the profile in NexaX, and print on your LSPc system.
Wash
Clean in xClean, then IPA — no more than 2 minutes in xClean or 5 minutes in IPA.
Cure
UV post-cure, then an optional 3-hour 150 °C thermal treatment for peak fire and heat performance.
Technical specifications
Values from the Nexa3D xPRO9400-FR TDS (2024 v5), fully post-cured. Highest HDT figures require the optional 3-hour 150 °C thermal post-treatment; UL 94 V-0 applies at 2 mm.
| Property | Value | Method |
|---|---|---|
| UL 94 flammability | V-0 (2 mm), V-1 (1.5 mm) | UL 94 |
| Limiting oxygen index | ≥ 28 | ISO 4589-2 |
| Rail fire classification | HL1 / HL2 | DIN EN 45545-2 |
| Tensile strength | 71–78 MPa | ASTM D638 |
| Tensile modulus | up to 4060 MPa | ASTM D638 |
| Elongation at break | 2.4–3.1 % | ASTM D638 |
| Flexural strength | 115 MPa | ASTM D790 |
| Flexural modulus | 3400 MPa | ASTM D790 |
| Izod impact, notched | 20 J/m | ASTM D256 |
| Hardness | 88 Shore D | ASTM D2240 |
| HDT @ 1.82 MPa | up to 141 °C | ASTM D648 |
| HDT @ 0.45 MPa | up to ~250 °C | ASTM D648 |
| Glass transition (Tg) | 175 °C | ASTM D4065 |
| Viscosity @ 25 °C | 830 cP | ASTM D7867 |
| Liquid density | 1.21 g/cm³ | ASTM D4052 |
Typical applications
Where fire performance and heat both matter.
Not sure xPRO9400-FR is the right resin?
Compare other Nexa3D LSPc engineering resins in our catalog.
Why source through Additive Plus
- Genuine Nexa3D resin from US stock — lot-consistent material, no grey-market repackaging.
- LSPc workflow support — validated NexaX profiles, wash, cure, and thermal post-cure dialed in.
- Volume pricing and official purchase orders — request a quote for 10 kg or more.
- Under 24h response from engineers who run these machines in-house.
| Brand | Nexa3D |
| Weight | 1.5 kg |
| Country of origin | USA |
| Printing Materials | Resins |
| Platform | XiP |
| Technology | LSPc |
| Resin Type | High-temp, Rigid |
| Application | Engineering, Manufacturing |
Send us your STL and we'll print a paid benchmark part in xPRO9400-FR in California — printed, cured to the flame-rated schedule, and shipped to you for fit and burn evaluation.
Common questions
Don't see yours? Email [email protected] — NDA standard, typical reply within 4 hours.
What exactly does the UL 94 V-0 rating on xPRO9400-FR cover?
Which Nexa3D printers run the 1.5 kg xPRO9400-FR cartridge?
What post-processing does xPRO9400-FR need to reach its published properties?
What applications is xPRO9400-FR intended for?
Is xPRO9400-FR halogen-free?
How should the cartridge be stored, and can I keep a part cartridge?
Can I order several cartridges or raise an official purchase order?
Place your order, or talk to an engineer first
Order Nexa3D xPRO9400-FR Flame-Retardant Engineering Resin – UL 94 V-0 at 2 mm | 1.5 kg direct, or talk to materials engineer