Mutual NDA on request before any file review. Talk to an engineer →
Metal powder · LPBF

A-Powder Inconel 718 Nickel Alloy Powder for LPBF — 15–53 µm, 10 kg

A-Powder Inconel 718 powder price: $835 per 10 kg ($83.50/kg)

Age-hardenable nickel superalloy with excellent strength at high temperature and good corrosion resistance. A-Powder is AO Metal's own powder brand, produced in China and sold and supported in the US by Additive Plus.

$835

Made to orderMade in China$83.50/kg
Made to order · 6–8 weeksExact date confirmed by email after you order
Premium grade · COA on request · Card, PayPal or PO
Request a formal quoteNew: 1 kg packs coming soon
Buying for a company?
Purchase orderAdd the quote number to your PO and send the PO to [email protected]. We invoice against your PO.
Tax-exemptChoose “Invoice” and upload your exemption or resale certificate at checkout, or send it with your PO.
New supplier setupW-9 and supplier forms on request.
COALot certificate on requestSDSSafety data sheet on request
NDA on request Ships in 6–8 weeks
15–53 µmParticle size
≤ 20 s / 50 gHall flow
≥ 1458 MPaUTS after heat treatment
≥ 80%Sphericity
ChinaCountry of origin
10 kgSealed container

Values from the manufacturer data for A-Powder Inconel 718. Catalog figures are minimums or ranges; the certificate for your lot is available on request.

Same alloy, 4 options

Which Inconel 718 is right for your build?

All of them are in our catalog at a published price. Pick by machine, timing and country of origin.

PowderParticle sizeOriginAvailabilityGood fit for10 kg
Carpenter Additive 718 F powder, 10 kg containerCarpenter Additive 718 FFine cut
15–45 µm · LPBFUSAIn stockPrograms that need a named mill and fast delivery$1,000View
Carpenter Additive 718 E powder, 10 kg containerCarpenter Additive 718 ECoarse cut
45–106 µm · DED, EBMConfirmed per lotIn stockDirected energy deposition and electron-beam systems$575View
CNPC Powder Inconel 718 powder, 10 kg containerCNPC Powder Inconel 718Named manufacturer
15–53 µm · LPBFChinaMade to orderR&D and cost-driven builds that can wait$900View
A-Powder Inconel 718 powder, 10 kg containerA-Powder Inconel 718This page
15–53 µm · LPBFChinaMade to orderLower LPBF price per kg, made to order$835Add to cart

Need a specific country of origin for a government or defense program? Ask before ordering and we will confirm it in writing for your lot.

Powder data

What is in the container

Specification from the manufacturer. The certificate for your lot is available on request.

Specification

Chemistry, manufacturer data for A-Powder Inconel 718 (wt%). The certificate for your lot lists all measured elements.

Elementwt%
Nickel (Ni)50.0–55.0
Chromium (Cr)17.0–21.0
Niobium (Nb)4.75–5.5
Molybdenum (Mo)2.8–3.3
Iron (Fe)Balance
Powder propertyRequirement
D10 / D50 / D9010–25 / 25–40 / 40–60 µm
Hall flow≤ 20 s / 50 g
Apparent / tap density≥ 3.5 / ≥ 4.0 g/cm³
Sphericity≥ 80%

What comes with your lot

From the manufacturer certificate

  • Chemistry against the specification limits on the left
  • Particle size distribution: D10, D50, D90
  • Flow rate and apparent density
  • Lot number for traceability

The certificate for your lot is available on request. The manufacturer datasheet for this alloy has no particle image; ask us if you need one.

Printed properties

How the printed metal performs

Printed-property minimums from the manufacturer data for A-Powder Inconel 718. A guide for your own qualification, not design data.

ConditionOrientationYield, MPaUTS, MPaElongationRel. densityHardness, HV1
As-built—≥ 829≥ 1049≥ 27%99.82%286
1065 °C 8 h + 720 °C 4 h + 620 °C 4 h—≥ 1307≥ 1458≥ 17%—530

Heat treatment

Manufacturer data

  • Heat treatment in the catalog data: 1065 °C for 8 hours, then 720 °C for 4 hours and 620 °C for 4 hours.
  • Use the solution, aging and HIP cycle your specification calls for, for example AMS5662.

Before you order

Ship date: confirmed by email after you order. If it does not work for you, we cancel the order and refund it in full.

Comparison

How this Inconel 718 compares

Published tensile data, X–Y direction unless noted, one representative condition per alloy. Conditions differ, so use this to shortlist, not to design.

AlloyConditionYield, MPaUTS, MPaElongationChoose it for10 kg
Inconel 7181065 °C 8 h + 720 °C 4 h + 620 °C 4 h (manufacturer data)≥ 1307≥ 1458≥ 17%Lowest price per kg$835
Inconel 625Stress relieved648100741%Corrosion resistance; cryogenic to 1093 °C (2000 °F)$1,160
Hastelloy XSolution + age39381641%Oxidation resistance to 1204 °C (2200 °F)$1,125
Compatibility and handling

Will it run on my printer?

Runs on open-parameter laser powder bed fusion systems with Inconel 718 parameters. Our materials engineer shares recommended starting parameters that you tune on your machine.

EOSM 290 · M 300-4 · M 400
SLM Solutions / NikonSLM 280 · 500
RenishawAM 400 · RenAM 500
DMG Mori · TRUMPFLasertec · TruPrint
Xact MetalXM series
Velo3D · Aconity3DSapphire · MIDI / ONE
3D Systems · BLT · Eplus3DDMP Flex / Factory · BLT-S · EP-M
and other open-parameter LPBFtuned per machine

Machine names identify compatible equipment only. Additive Plus is not affiliated with these manufacturers, and the powder is not approved by them. Process parameters are tuned per machine.

Step 1

Store sealed

Keep the container closed, dry and at room temperature until you load the printer.

Step 2

Sieve

Sieve before loading and every time you reuse powder recovered from a build.

ATO Sieve ultrasonic metal powder sieving stationATO Sieve · quote
Step 3

Load and purge

Fill the dispenser, close the chamber and purge with argon or nitrogen.

Step 4

Print and relieve

Stress-relieve on the plate, then remove parts and supports.

Step 5

Recover

Collect unfused powder, sieve it and return it to a sealed container.

Delfin Mistral 451 BL D2 — ATEX metal powder vacuumDelfin Mistral 451 BL D2 — ATEX metal powder vacuum · $7,175

Wear a respirator, gloves and eye protection when handling metal powder. Read the safety data sheet before first use.

Applications

Printed on AO Metal

Real builds on the LPBF printers we sell, and what teams make from this alloy.

Recoater spreading 316L powder while the laser melts a grid of test cubes on an AO Metal printer
Powder in the chamberThe recoater spreads 316L powder, then the laser melts a grid of test cubes.
Stainless steel test cubes and lattice coupons printed on the AO Metal A30, measured with a caliper
Test cubes and latticesStainless steel coupons printed on the AO Metal A30, checked with a caliper.
Lattice cube printed on the AO Metal A30 build plate
Lattice on the plateA lattice cube on the AO Metal A30 build plate.
Metal heat exchanger printed on the AO Metal A100
Heat exchangerPrinted on the AO Metal A100; LEAP 71 reference geometry.

Parts printed on AO Metal printers, which we sell. Alloys, parameters and powder lots differ from part to part; these photos show the process, not parts made from this specific powder lot.

  • Turbine and engine parts
  • Hot-section aerospace parts
  • Industrial high-temperature parts

Applications as listed in the manufacturer data for A-Powder Inconel 718.

Ordering

Ordering, delivery and our promise

Pack

A sealed 10 kg container of 15–53 µm powder, with the certificate of analysis for the lot on request.

Delivery

The ship date shows next to the Add to Cart button. Shipping cost is calculated at checkout.

Payment

Card or PayPal at checkout, an invoice, or a purchase order — choose how you buy next to Add to Cart.

Volume

100 kg and more: ask for a volume quote with your alloy, quantity and ship-to.

If the powder is not right, we make it right.

If your lot’s chemistry or particle size falls outside its certificate or this page, or it arrives damaged or wrong, tell us within 14 days of delivery. We replace it or refund you, and we pay for shipping both ways.

Frequently bought together

Complete the workflow

EOS M290 SS316 Build Plate | 50mm Corrosion-Resistant LPBF Platform
Engineering
EOS M290 SS316 Build Plate | 50mm Corrosion-Resistant LPBF Platform
316L stainless steel build plate for EOS M280/M290 LPBF systems. 9.92×9.92×1.97in (252×252×50mm) profile, CNC-machined and ground flat for consistent stainless and tool-steel builds.
  • ✓ 316L — stronger pitting and chemical resistance than 304 stainless
  • ✓ Precision-ground flatness for consistent first-layer adhesion
  • ✓ Made to order — choose your speed below: Express 2–3 wks, or Standard 6–8 wks (save ~45%)
From $720
Get quote
Express 2–3 wks · Standard 6–8 wks
Delfin Mistral 451 BL D2 ATEX Combustible-Dust Vacuum – Non-Reactive Metal Powder | 12 gal
Additive Manufacturing Solutions
Delfin Mistral 451 BL D2 ATEX Combustible-Dust Vacuum – Non-Reactive Metal Powder | 12 gal

ATEX-certified industrial vacuum for combustible dust and non-reactive metal powder — built to the D2 standard for Zone 22 areas, with antistatic, grounded construction and a Class M filter. 2 kW, 3-inch inlet, 12-gallon container.

  • ✓ Conductive / antistatic build — no static build-up around ignition-sensitive powder
  • ✓ For stainless, nickel & non-reactive AM powder — reactive metals need the inert unit
  • ✓ In US stock · ships in 2–3 business days · genuine Delfin unit · ATEX docs on request
From $7175
Add to cart
2–3 Business Days
AM Solutions S1 — Automated Depowdering & Surface Finishing System
Depowdering stations
AM Solutions S1 — Automated Depowdering & Surface Finishing System

Automated 2-in-1 blasting cell that depowders and surface-finishes powder-bed 3D-printed parts in one enclosed, software-controlled cycle.

  • ✓ Depowdering + surface finishing in one ATEX-compliant cell
  • ✓ Polymer PBF (SLS, MJF, HSS, SAF) + de-powdered metal parts
  • ✓ Lead time: 4–8 weeks — built to order · install + training included
For Cleaning, Surface finishing
From $69920
Add to cart
Ships in 4–8 weeks — built to order. Install and operator training included.
IN625 Nickel Alloy Powder for Metal 3D Printing | LPBF Compatible - 10 kg / 22 lbs
LPBF (DMLS) 3D Printing Materials
IN625 Nickel Alloy Powder for Metal 3D Printing | LPBF Compatible - 10 kg / 22 lbs

High-temp. Corrosion-proof. Non-magnetic. Genuine Carpenter PowderRange® 625 (Inconel® 625) nickel superalloy for LPBF, EBM & DED metal 3D printing.

  • ✓ Strength & corrosion resistance to 2000°F (1093°C)
  • ✓ Sold in small, workable volumes — no large mill minimums
  • ✓ COA on request
For Metal LPBF
From $1160
Get quote
Ship date confirmed after you order
1 / 1
Not ready for a full bottle? Request a sample or a custom quantity.

Common questions

Don't see yours? Email [email protected] — NDA on request.

What is A-Powder Inconel 718 nickel alloy powder?
A-Powder Inconel 718 nickel alloy powder is an age-hardenable nickel superalloy with excellent strength at high temperature and good corrosion resistance. It is a 15–53 µm cut for laser powder bed fusion, with 50.0–55.0% nickel, 17.0–21.0% chromium, 4.75–5.5% niobium and 2.8–3.3% molybdenum, with iron as the balance. Typical uses listed by the manufacturer include turbine and engine parts, including the hottest sections, in aerospace and industry.
What strength does printed Inconel 718 nickel alloy reach with this powder?
According to the manufacturer data, as-built parts reach at least 829 MPa yield and 1,049 MPa tensile strength with 27% elongation and 99.82% relative density. After 1065 °C for 8 hours, 720 °C for 4 hours and 620 °C for 4 hours, the catalog lists at least 1,307 MPa yield, 1,458 MPa tensile and 17% elongation. These are minimum values from the data sheet, not design data, so qualify the alloy on coupons from your own machine and parameters.
How is Inconel 718 nickel alloy heat treated after printing?
The catalog lists properties after 1065 °C for 8 hours, then 720 °C for 4 hours and 620 °C for 4 hours, which raised tensile strength to at least 1,458 MPa. Many programs use the AMS5662 solution and aging cycle instead. Follow your specification and qualify the cycle on coupons from your machine. Our materials engineer can help you plan test coupons and starting parameters before your first production build.
What particle size and flow does A-Powder Inconel 718 nickel alloy powder have?
A-Powder Inconel 718 nickel alloy powder is a 15–53 µm cut. The manufacturer data specifies D10 of 10–25 µm, D50 of 25–40 µm and D90 of 40–60 µm, Hall flow of 20 s per 50 g or less, apparent density of at least 3.5 g/cm³ and sphericity of at least 80%. The certificate of analysis for your lot reports the measured particle size distribution and chemistry, and it is available on request.
Who makes A-Powder Inconel 718 nickel alloy powder?
A-Powder is AO Metal's own brand of laser powder bed fusion powders, produced in China under an ISO 9001 quality system and sold and supported in the US by Additive Plus. Each container is traceable to its lot, and the certificate of analysis with chemistry and particle-size data is available on request.
How is A-Powder Inconel 718 nickel alloy powder different from PowderRange 718 from Carpenter Additive?
Both are listed in the table at the top of this page with their prices, particle size and availability. A-Powder Inconel 718 nickel alloy powder is made in China and is the lower-priced option per kilogram, while PowderRange 718 from Carpenter Additive comes with a named mill's published datasheet and ships from US stock when available. Choose by your program's country-of-origin rules, budget and timing.
How do I order A-Powder Inconel 718 nickel alloy powder, and when does it ship?
Add it to the cart and pay by card or PayPal, choose Invoice me at checkout to receive an invoice for bank transfer, or send a purchase order to [email protected]. After you order, we confirm availability and the ship date by email. If that date does not work for you, we cancel the order and refund it in full. For 100 kg or more, ask us for a volume quote.

Place your order, or talk to an engineer first

Order A-Powder Inconel 718 Powder for Metal 3D Printing | 15–53 µm LPBF – 10 kg / 22 lbs direct, or talk to materials engineer

Add to cart