A-Powder Inconel 718 Nickel Superalloy Powder for Metal 3D Printing | LPBF Compatible – 10 kg / 22 lbs
$1,090
High-Temperature Strength. Corrosion-Resistant.. High-performance Inconel 718 powder for LPBF additive manufacturing. Heat-resistant, corrosion-resistant, and fully heat-treatable for aerospace, energy, and industrial high-temperature components. OEM-optimized Inconel 718 powder for metal 3D printing, delivering reliable prints, predictable LPBF performance, and full traceable documentation.
-
Technology:
Metal LPBF
-
Printing Materials:
Metal Powders
-
Production Method:
Vacuum Induction Melting Gas Atomization (VIGA)
-
Powder Package:
10 kg bottle, 440 kg hopper, 840 kg hopper
Need more than 100 kg / 222 lbs? Or official request?
OEM-Optimized Supply — Powered by Additive Plus
✔ Application-driven material engineering and validation
✔ Optimized printing parameters for maximum performance
✔ Reduced trial-and-error through pre-qualified solutions
✔ Improved repeatability and process stability
✔ Developed for demanding industrial use cases
| Quantity, kg | Per Bottle 10 kg | Per kg |
|---|---|---|
| 10-100 | $1090.00 | $109.00 |
| 100+ | $980.00 | $98.00 |
- Description
- Details
- Materials
- FAQ
- Documents
- Videos
- Review
Description
A-Powder Inconel 718 Nickel Superalloy Powder is a premium nickel-based superalloy designed for LPBF additive manufacturing. Produced via vacuum induction gas atomization (VIGA), the powder features spherical morphology, tight particle size distribution (15–53 µm), and ultra-low oxygen content (≤200 ppm). This ensures smooth recoating, predictable flow, and repeatable layer fusion. The alloy composition (Ni 51.7 %, Cr 20.06 %, Fe balance, Nb 5.01 %, Mo 3.17 %, Ti 1.02 %, Al 0.47 %) provides excellent high-temperature strength and corrosion resistance. Heat treatment achieves ultimate tensile strength 1350 MPa, yield strength 1150 MPa, and elongation 23 %, making A-Powder Inconel 718 ideal for aerospace, energy, and critical industrial applications. Small-batch flexibility, rapid delivery, and full traceable documentation from AO Metal guarantee production-ready performance.
| Element | Min | Max | Typical |
| Fe | Bal. | Bal. | Bal. |
| Cr | 15.0 | 17.0 | 16.28 |
| Cu | 3.0 | 5.0 | 4.15 |
| Ni | 3.0 | 5.0 | 4.18 |
| Nb+Ta | 0.15 | 0.45 | 0.28 |
| Si | – | 1.0 | 0.49 |
| Mn | – | 1.0 | 0.20 |
| C | – | 0.07 | 0.006 |
| P | – | 0.02 | 0.006 |
| S | – | 0.02 | 0.004 |
| O | – | 0.08 | 0.030 |
| N | – | 0.15 | 0.015 |
machine type: F – LPBF INDUSTRIES: Aerospace / Energy / Industrial
Key Performance Benefits
- High-temperature nickel-based superalloy with excellent corrosion resistance
- Predictable LPBF performance with stable layer deposition
- Spherical particle morphology ensures repeatable powder flow
- Heat-treatable for optimized mechanical properties
- Suitable for complex, high-temperature, end-use components
Typical Applications
- Aerospace turbine and structural components
- High-temperature energy and power system parts
- Industrial machinery requiring corrosion resistance and strength
- Precision end-use components for critical applications
- Brand AO Metal – High-Precision Metal 3D Printers for Innovation
- Technology Metal LPBF
- Powder Package 10 kg bottle, 440 kg hopper, 840 kg hopper
- PSD (particle size distribution) 15–53 μm
- Printing Materials Metal Powders
- Material IN718
- Country of origin China
- Production Method Vacuum Induction Melting Gas Atomization (VIGA)
Materials
Applicable Standards: ASTM F3055, ASTM B213, ASTM B212, ASTM B527, ISO13320
Manufacturing Method: Vacuum Induction Melting Gas Atomization (VIGA).
Particle Shape: Spherical.
- IN718
Frequently asked questions
What is Inconel 718?
Inconel 718 is a nickel-based superalloy powder engineered for LPBF additive manufacturing. It provides excellent high-temperature strength, corrosion resistance, and predictable mechanical performance after heat treatment.
Which additive manufacturing processes are compatible?
Optimized for LPBF. Spherical particles with tight PSD (15–53 µm) and ultra-low oxygen content (≤200 ppm) provide smooth recoating, minimal spatter, and repeatable layer deposition.
Can Inconel 718 be heat-treated?
Yes, heat treatment improves mechanical properties: UTS 1350 MPa, yield 1150 MPa, elongation 23 %, hardness 45 HRC.
What industries typically use Inconel 718?
Aerospace, energy, and industrial applications requiring high-temperature, corrosion-resistant, and structurally critical components.
Documents
Videos